薄 膜 性 能
|
測試方法
|
單位
|
典型數(shù)值
|
|
厚 度 |
ASTM D 2673 |
μm
|
25
|
|
密 度 | ASTM D 792 |
g/cm3
|
0.90
|
|
鋁層厚度 | SJ Method |
Ω/□
|
1.6
|
|
拉伸強(qiáng)度 |
MD |
ASTM D 882 |
MPa
|
49.2
|
TD
|
35
|
|||
斷裂伸長率 |
MD
|
ASTM D 882 |
MPa
|
578
|
TD
|
718
|
|||
摩擦系數(shù) |
u/u
|
ASTM D 1984 |
——
|
0.7
|
表面張力 | GB/T14216-93 |
Dyne/cm
|
38
|
|
起封溫度 |
u/u
|
SJ Method
條件:2.0kgf/cm2,1.0sec,8.0N/15mm
|
℃
|
128
|
鋁層附著力 | SJ Method |
%
|
96
|
|
水蒸汽氣透過率 |
ASTM F 1249
條件:38℃-90%RH
|
g/m2/24h
|
1.20
|
|
氧氣透過率 |
ASTM D 3985
條件:23℃-0%RH
|
cc/m2/24h
|
20.0
|